Cover of Portland Cement: Stone, Fire, Concrete, a book by Ketineni RamaraoFrom the book Portland Cement: Stone, Fire, Concrete
Chapters 11, 14, 15 and 16. Read the full book free as a PDF.
Diagram of the six steps of making Portland cement: quarry, crush, grind and blend, preheat and kiln, cool to clinker, and grind with gypsum.
The route from rock to cement. Original IOI diagram, steps from the American Cement Association and the US EPA.

Start with rock

Portland cement is made from four main elements: calcium, silicon, aluminium and iron. Limestone, marl and clay are the usual sources. Other materials can fill in, including shells, chalk, shale, slate, silica sand, iron ore and blast furnace slag. Plants quarry limestone, clay and sand, and many also add by-products such as fly ash and slag as alternative raw materials.

Crush, test, grind, blend

The rock is broken into baseball-size pieces and samples go to a laboratory for analysis. The fragments are then finely ground and combined with clay, shale, iron ore and the other ingredients. Small quantities of iron ore, alumina and other minerals can be added to adjust the composition. Some manufacturers grind the raw materials dry. Others use wet grinding with water. That choice splits the industry into the two kiln families covered in dry process versus wet process cement kilns.

Black and white photograph looking up at two huge horizontal cylindrical rotary kilns on steel supports inside a cement plant, with metal walkways and railings in the foreground.
Rotary kilns at the Sundon cement plant, Bedfordshire, England. The kiln is a long, slightly inclined steel cylinder that turns slowly while the raw mix moves toward the flame. Photo: Dylan Moore, CC BY-SA 2.0, via Geograph and Wikimedia Commons.

The kiln

The blended material goes first through a preheater tower, which uses heat generated by the plant to start the chemical reactions and so makes the kiln more efficient. Then it enters the upper end of the kiln. The US EPA describes a rotary kiln as roughly 20 to 25 feet in diameter and from 150 feet to well over 300 feet long, set at a slight incline and rotating one to three times a minute. The flame sits at the lower end, and the raw material moves toward it as the kiln turns. The material reaches temperatures from 2,500 degrees Fahrenheit to well above 3,000. The American Cement Association gives about 2,700 degrees Fahrenheit, which the ACA says makes the material partially molten.

Three things happen in the kiln, according to the EPA. First, all moisture is driven out. Second, the calcium carbonate in limestone dissociates into carbon dioxide and calcium oxide, free lime, in a step called calcination. Third, the lime and the other minerals react to form calcium silicates and calcium aluminates, the main components of clinker. This last step is called clinkering or sintering.

Clinker

Two small dark grey rough spheres of cement clinker, about the size of marbles, sitting on a polished wooden surface.
Two pieces of clinker. Clinker leaves the kiln as grey balls about the size of marbles and is then ground with gypsum to make cement. Photo: Lorenzo Bonino, CC BY 3.0, via Wikimedia Commons.

Clinker leaves the kiln as grey balls about the size of marbles. It comes out red-hot, with a consistency like a lava flow, and is cooled quickly in a clinker cooler that returns the heated air to the kiln to save fuel. The EPA adds a reason for the speed: rapid cooling limits the formation of a glass phase and gives the maximum yield of alite, tricalcium silicate, an important component for the hardening properties of cement.

Final grinding, with gypsum

A ball mill grinds the clinker with gypsum or other ingredients into fine cement. The American Cement Association puts the fineness at about 150 billion grains per pound. The EPA gives the usual gypsum addition as approximately 5 percent, to control the setting properties of the cement. After that the cement goes to be used, mostly as the binder in concrete.

Where the energy and carbon sit

The EPA says essentially all greenhouse gas emissions from cement manufacturing are CO2 from clinker production, and that finish grinding adds no direct process CO2 from calcination, though it uses electricity that can cause indirect emissions. They come from two sources: the fuel burned in the kiln, and the calcination reaction itself. Blending higher ratios of limestone or supplementary cementitious materials into the cement can reduce a plant's carbon footprint by up to 10 percent, according to the American Cement Association. Plants also co-process alternative fuels such as tyre-derived fuel, which the same source says supplies more than 15 percent of the energy used by US cement plants.

The process is simple to state and hard to change. Limestone has to lose its CO2 for cement chemistry to work, which is why the process emissions are separate from the fuel question. This is the thread the book follows from the quarry to the kiln.

Quick answers

How is Portland cement made?

Limestone, clay and other materials are quarried, crushed, ground and blended, preheated, then fired in a rotary kiln to about 2,700 degrees Fahrenheit. The product, clinker, is cooled and ground with gypsum into cement.

What is clinker?

The grey, marble-sized balls that leave the kiln. They are made of calcium silicates and calcium aluminates and are ground with gypsum to make cement.

Why is gypsum added to cement?

The EPA says approximately 5 percent gypsum is added to control the setting properties of the cement.

Where do cement plants' CO2 emissions come from?

Essentially all of them come from clinker production: fuel burned in the kiln and the calcination reaction that releases CO2 from limestone. Finish grinding produces no direct process emissions, according to the EPA; it does use electricity, which carries indirect emissions.

Sources

Process steps and the 150 billion grains per pound figure are from the American Cement Association. Kiln dimensions, the three kiln reactions, rapid cooling, the 5 percent gypsum figure and emissions sources are from the US EPA. The ACA and EPA give slightly different temperature descriptions (about 2,700 F versus 2,500 to above 3,000 F) and both are reported.

More from this book

Types · From the book Portland Cement: Stone, Fire, Concrete

Types of Portland cement: Type I to V, blended and performance cements

There is no single thing called cement on a construction site.

Explainer · From the book Portland Cement: Stone, Fire, Concrete

Cement vs concrete: how concrete is made

People say cement when they mean concrete.

History · From the book Portland Cement: Stone, Fire, Concrete

Who invented Portland cement? Aspdin, Smeaton and a long argument

The usual answer is Joseph Aspdin, a Leeds bricklayer, in 1824.

Technology · From the book Portland Cement: Stone, Fire, Concrete

Dry process vs wet process: why cement kilns changed

A cement kiln has to drive off water, split limestone into lime and carbon dioxide, and then fuse the result.